| Aspect | Air Drying | Kiln Drying | |--------|-----------|--------------| | Time | Months to years | Days to weeks | | Final MC | 12–16% (climate dependent) | 6–10% (adjustable) | | Cost | Low (space, stickers) | High (equipment, energy) | | Defect risk | Mold, stain, insects | Casehardening, collapse, honeycomb | | Best for | Large timbers, local use, low budget | Furniture, flooring, export, precision |

This method is slow, often taking several months to over a year, depending on the wood species and thickness. seasoning timber