Once the SSD condition is achieved, the procedure proceeds as follows:
Drying: Dry the sample to a constant mass in an oven at 110°C. Once the SSD condition is achieved, the procedure
Achieving SSD State: Use a hair dryer or gentle air current to dry the aggregate until it reaches a free-flowing "SSD" state, verified by the Cone Test. Once the SSD condition is achieved